Credit: Stephen Raiman/Oak Ridge National Laboratory, U.S. Dept. of Energy
At the salt–metal interface, thermodynamic forces drive chromium from the bulk of a nickel alloy, leaving a porous, weakened layer. Impurities in the salt drive further corrosion of the structural material.